| Temper: Nominal Grain Size 0.025 mm Fabrication Properties: Excellent Suitability – Soldering, Brazing, Capacity for Being Cold Worked; Good Suitability – Oxyacetylene Welding, Gas Shielded Arc Welding, Butt Weld; Fair Suitability – Capacity for Being Hot Formed Common Fabrication Processes: Blanking; Drawing; Forming; Piercing Typical Uses: Weather Stripping; Pen Clips; Connectors; Electrical Connectors; Fuse Clips; Switch Springs; Switches; Terminals; Bushings; Contact Springs Applicable Specifications: Bar – ASTM B591; Plate – ASTM B591; Sheet - ASTM B591; Strip – ASTM B888/B88M, ASTM B591 |