MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Ethydco Advancene™ EM-4810-AAH HDPE Blow Molding Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: Blow molding. A polymer with broad molecular weight distribution and high molecular weight. This product provides an excellent combination of extrudability and parison stability, which contribute to uniform wall thickness in large parts. It is ideal for blow molding containers of >80 liters closed head shipping containers and other similar parts. The broad distribution also provides outstanding environmental stress crack resistance at a good rigidity. Because of these characteristics, a wide variety of products, such as industrial chemicals, latex paints, printing inks, foodstuffs, adhesives, and other chemical specialties my be packaged in containers produced from this resin. The smooth surface of molded parts is readily treated and printed for high quality applications. Main characteristics: outstanding environmental stress crack resistance, excellent parison melt strength/low sag, good extrudability/processability, good rigidity.

Mechanical property data for samples molded and tested in accordance with ASTM D4976.

Information provided by ETHYDCO.

Vendors:
Available Properties
  • Density, ASTM D792
  • ESCR 100% Igepal®, ASTM D1693, F50
  • High Load Melt Index, ASTM D1238, ISO 1133
  • Hardness, Shore D, ASTM D2240, ISO/IEC 17025:1999
  • Tensile Strength at Break, ASTM D638, ISO 527
  • Tensile Strength, Yield, ASTM D638, ISO 527
  • Elongation at Break, ASTM D638, ISO 527
  • Elongation at Yield, ASTM D638, ISO 527
  • Flexural Modulus, ASTM D790B, ISO 178,
  • Tensile Impact Strength, ASTM D1822, ISO 8256, Type S
  • Melting Point, ASTM D3418, ISO 3146
  • Crystallization Temperature, ASTM D3418, ISO 3146
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648, ISO 75, Unannealed
  • Vicat Softening Point, ASTM D1525, ISO 306
  • Brittleness Temperature, ASTM D746, ISO 974( E)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.