MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
LyondellBasell Hifax CA 387 A Thermoplastic Polyolefin
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Hifax polypropylene resins based on the Catalloy process are used in applications such as building and construction (e.g., single-ply roofing), industrial applications (e.g., wire and cable), and automotive industries. Hifax priovides good processability, excellent impact resistance, a broad range of stiffness from very soft to rigid products, high temperature resistance and low linear coefficient of thermal expansion.

Hifax CA 387 A is a reactor TPO (thermoplastic polyolefin) manufactured using LyondellBasell's proprietary Catalloy process technology. It has high melt flow and an excellent balance of impact, stiffness, processability and paintability. Hifax CA 387 A is primarily used for painted automotive bumper fascias that require high durability, and for other injection molded parts with paintable and weatherable requirements. It is also utilized as a component in compounded materials for a wide range of industrial applications. The grade is available in natural pellet form. Applications: Bumpers, Caps & Closures, Exterior Automotive Applications, Interior Automotive Applications, Polymer Modifier.

Information provided by LyondellBasell.

Vendors:
Available Properties
  • Density, ISO 1183-1, method A
  • Melt Flow, ISO 1133-1
  • Hardness, Shore D, ISO 868
  • Tensile Strength at Break, ISO 527-1,-2
  • Tensile Strength, Yield, ISO 527-1,-2
  • Elongation at Break, ISO 527-1,-2
  • Elongation at Yield, ISO 527-1,-2
  • Flexural Modulus, ISO 178
  • Charpy Impact, Notched, ISO 179, failure mode- complete break
  • Charpy Impact, Notched, ISO 179, failure mode- complete break
  • Charpy Impact, Notched, ISO 179, failure mode-partial break
  • Impact Test, ASTM D 3763, Multi-axial Impact Strength, 2.2m/s,3.2mm plaque, failure mode: ductile
  • Impact Test, ASTM D 3763, Multi-axial Impact Strength, 2.2m/s,3.2mm plaque, failure mode: ductile
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75B-1,-2, unannealed
  • Vicat Softening Point, ISO 306, A50
  • DSC Induction Temperature, ISO 11357-3
  • Gloss, ASTM D2457, 60°
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
LyondellBasell LYB (former Equistar)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.