| Hexene Copolymer Linear Medium Density Polyethylene. This resin is fully UV8 stabilized. High quality Polyethylene compound specially designed for automotive applications, water tanks, diesel tanks and those applications requiring very good mechanical properties, bubble-free parts and smooth surface finish. Meets CONEG regulation for articles intended for direct food contact. Information provided by Polimeros Mexicanos |