| PEEK tribologically modified with 20 % PTFE Properties: dimensionally stable, good gliding properties, good aging behavior, good fire behavior, High strength, High wear resistance, Very high continuous used temperature, semi-crystalline Typical areas of application: Fasteners, Housing, Sliding elements, Piston, Rotors, Bobbin, Plug, Valves, Gears Industries: Automotive, Electrical and electronics industry, Household appliances, Aviation Industry, Mechanical Engineering, Medical Technology Information provided by BARLOG plastics GmbH. |