MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Propex Fabrics Curv™ C100A Polypropylene/Polypropylene Thermoformable Composite
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Curv™ key features include weight savings, total recyclability, no glass content, thermoformable, high impact strength, inertness, and abrasion resistance.

Data provided by BP Amoco; Curv was spun off from BP Amoco in 2004 and is now a product of Propex Fabrics.

Vendors:
Available Properties
  • Density, ASTM D792
  • Density, ISO 1183
  • Water Absorption, DIN 53495
  • Water Absorption, ASTM D570-81, 20°C
  • Water Absorption, ASTM D570-81, 100°C
  • Ball Indentation Hardness, EN ISO 2039-1
  • Tensile Strength, Ultimate, DIN EN ISO 527, MD
  • Tensile Strength, Ultimate, DIN EN ISO 527, CD
  • Tensile Strength, Ultimate, ASTM D638M-92
  • Elongation at Break, ASTM D638M-92
  • Elongation at Break, DIN EN ISO 527, MD
  • Elongation at Break, DIN EN ISO 527, CD
  • Tensile Modulus, DIN EN ISO 527, MD
  • Tensile Modulus, DIN EN ISO 527, CD
  • Tensile Modulus, ASTM D638M-93
  • Flexural Strength, DIN EN ISO 178, MD
  • Flexural Strength, DIN EN ISO 178, CD
  • Flexural Strength, ASTM D790M-93
  • Flexural Modulus, DIN EN ISO 178, MD
  • Flexural Modulus, DIN EN ISO 178, CD
  • Flexural Modulus, ASTM D790M-93
  • Compressive Strength, EN ISO 604, Normal to Plane
  • Izod Impact, Notched, ASTM D256-93a
  • Izod Impact, Notched, ASTM D256-93a
  • Izod Impact, Notched (ISO), EN ISO 180/2 ep b, 22 J
  • Izod Impact, Notched (ISO), EN ISO 180/2 ep b, 22 J
  • Izod Impact, Unnotched (ISO), EN ISO 180/2 ep, 22 J
  • Charpy Impact Unnotched, EN ISO 179/2 ep
  • Charpy Impact Unnotched, EN ISO 179/2 ep, Low Temp
  • Charpy Impact, Notched, EN ISO 179/2 ep b
  • Tensile Impact Strength, EN ISO 8256, MD
  • Tensile Impact Strength, EN ISO 8256, CD
  • Puncture Energy, ASTM D3763-97a, 70°C High Speed Puncture Energy
  • Puncture Energy, ASTM D3763-97a, 100°C High Speed Puncture Energy
  • Puncture Energy, ISO 6603, Puncture Impact; 52 J; 2.1 mm
  • Puncture Energy, ASTM D3763-97a, High Speed Puncture Energy
  • Torsional Stiffness, DIN EN ISO 6721
  • CTE, linear, ASTM D696, Temp range not reported
  • CTE, linear, DIN 53752
  • Deflection Temperature at 0.46 MPa (66 psi), EN ISO 75-2B, flatwise
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648-82/88
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648-82/88
  • Deflection Temperature at 1.8 MPa (264 psi), EN ISO 75-2A, flatwise
  • Vicat Softening Point, DIN EN ISO 306, 50K/h
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.