| HE2595 is a black, molecular weight, high density polyethylene compound for crosslinkable pipes, especially designed for electron beam irradiation crosslinking. The stabilization package is optimized for good processability, easy crosslinking as well as service at high temperatures. Well dispersed carbon black gives outstanding UV resistance. Crosslinked pipes based on HE2595 are recommended for domestic hot and cold water supply, natural gas distribution, radiator connection, floor heating and industrial applications. Former trade name for this product was BorPEX™. Information provided by the Manufacturer. |