MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Eastman Tsunami GS1 Copolyester Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyester, TP

Material Notes: Tsunami copolyester is an Eastman Specialty Plastic developed for the calendering industry. It can be used on existing calendering lines with no or minimal modification. Tsunami copolyester is used for decorative lamination. This product is only available in Europe and Asia.

Applications/Uses

  • Laminating
  • This product, formerly sold under the 'Tsunami' name is now a part of Eastman's 'Cadence' product line.

    Vendors:
    Available Properties
    • Specific Gravity, ASTM D1505
    • Density, ASTM D1505, Film
    • Water Absorption, ASTM D570, 24h Immersion
    • Water Vapor Transmission, ASTM F372
    • Oxygen Transmission, ASTM D3985
    • Viscosity Measurement, EMN-A-AC-G-V-1, Inherent
    • Thickness
    • Film Tensile Strength at Yield, MD, ASTM D882
    • Film Tensile Strength at Yield, TD, ASTM D882
    • Film Elongation at Break, MD, ASTM D882
    • Film Elongation at Break, TD, ASTM D882
    • Film Elongation at Yield, MD, ASTM D882
    • Film Elongation at Yield, TD, ASTM D882
    • Tensile Modulus, ASTM D882, TD
    • Tensile Modulus, ASTM D882, MD
    • Puncture Energy, ASTM D3763, Puncture Resistance @Max Load, -30°C
    • Puncture Energy, ASTM D3763, Puncture Resistance @Max Load, 0°C
    • Puncture Energy, ASTM D3763, Puncture Resistance @Max Load, 23°C
    • Elmendorf Tear Strength, MD, ASTM D1922
    • Elmendorf Tear Strength, TD, ASTM D1922
    • Film Tensile Strength at Break, MD, ASTM D882
    • Film Tensile Strength at Break, TD, ASTM D882
    • Volume Resistivity, ASTM D257
    • Surface Resistivity per Square, ASTM D257
    • Dielectric Constant, ASTM D150
    • Dielectric Constant, ASTM D150
    • Dielectric Strength, ASTM D149, Short Time, 500V/sec
    • Dissipation Factor, ASTM D150
    • Dissipation Factor, ASTM D150
    • Arc Resistance, ASTM D495
    • CTE, linear, ASTM D696
    • Specific Heat Capacity, DSC
    • Specific Heat Capacity, DSC
    • Specific Heat Capacity, DSC
    • Specific Heat Capacity, DSC
    • Specific Heat Capacity, DSC
    • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
    • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
    • Vicat Softening Point, ASTM D1525
    • Glass Transition Temp, Tg, DSC
    • Oxygen Index
    • Haze, ASTM D1003
    • Gloss, ASTM D2457, at 60°
    • Transmission, Visible, ASTM D1003, Total Transmittance
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    Manufacturer Notes:
    Eastman Chemical Company

    Category Notes
    Plastic

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

     

    Proto3000 – 3D Engineering Solutions
    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.