| HD 54B04 is injection-molding grade high density polyethylene. Good high rigidity, easy processing, and UV resistance make it especially suitable for usage in crates, pallets, seats and Boxes. Application: Crates, Pallets, Boxes, Seats, Caps & closures. Features: Co-monomer Butene-1, High rigidity, UV resistant. Additives: Antioxidants, lubricant, Acid scavenger, UV stabilizer.Information provided by Persian Gulf Polymer - Pooya Tejarat Novin Co. |