MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Eastman Eastar A150 Copolyester, Film
Categories: Polymer; Film; Thermoplastic; Polyester, TP

Material Notes: Eastar A150 Copolyester is a poly(1,4-cyclohexylene-dimethylene terephthalate/isophthalate). It is produced by reacting terephthalic acid and isophthalic acid with the glycol 1,4-cyclohexanedimethanol. Eastar A150 is intended primarily for extrusion into film and sheeting for packaging applications. It has excellent hydrolytic stability and good heat stability. Eastar A150 copolyester is lawful for use in food contact applications under food additive regulations published at 21 CFR 177.1240 by the Federal Food and Drug Administration. Therefore, it is lawful for use as a packaging material for meat or poultry foods prepared under federal inspection of the U.S. Department of Agriculture regulations at 9 CFR 318.7 and 381.147.

Applications/Uses

  • Blister Packaging
  • Food Packaging
  • Food-contact applications
  • Rigid Medical
  • Vendors:
    Available Properties
    • Bulk Density, ASTM D1895, Poured
    • Bulk Density, ASTM D1895, Vibrated
    • Density, ASTM D1505
    • Water Vapor Transmission, ASTM F372
    • Oxygen Transmission, ASTM D3985
    • Carbon Dioxide Transmission, ASTM D1434
    • Viscosity Measurement, EMN-A-AC-G-V-1, Inherent, Film
    • Viscosity Measurement, EMN-A-AC-G-V-1, Inherent
    • Thickness, ASTM D374
    • Film Tensile Strength at Yield, MD, ASTM D882
    • Film Tensile Strength at Yield, TD, ASTM D882
    • Film Elongation at Break, MD, ASTM D882
    • Film Elongation at Break, TD, ASTM D882
    • Film Elongation at Yield, MD, ASTM D882
    • Film Elongation at Yield, TD, ASTM D882
    • Tensile Modulus, ASTM D882, TD
    • Tensile Modulus, ASTM D882, MD
    • Coefficient of Friction, ASTM D1894
    • Tear Strength, Total, ASTM D1938, Split Tear Method, 254mm/min, TD
    • Tear Strength, Total, ASTM D1938, Split Tear Method, 254mm/min, MD
    • Elmendorf Tear Strength, MD, ASTM D1922
    • Elmendorf Tear Strength, TD, ASTM D1922
    • Dart Drop, ASTM D1709, 23°C
    • Dart Drop, ASTM D1709, at -30°C
    • Dart Drop, ASTM D1709, at -18°C
    • Film Tensile Strength at Break, MD, ASTM D882
    • Film Tensile Strength at Break, TD, ASTM D882
    • Heat of Fusion, ASTM E793
    • Specific Heat Capacity, DSC
    • Specific Heat Capacity, DSC
    • Specific Heat Capacity, DSC
    • Specific Heat Capacity, DSC
    • Specific Heat Capacity, DSC
    • Melting Point, ASTM D3418, Crystalline Peak
    • Glass Transition Temp, Tg, ASTM D3418
    • Haze, ASTM D1003
    • Gloss, ASTM D2457, at 45°
    • Transmission, Visible, ASTM D1746, Transparency
    • Transmission, Visible, ASTM D1003, Regular Transmittance
    • Transmission, Visible, ASTM D1003, Total Transmittance
    • FDA, See notes for details.
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    Manufacturer Notes:
    Eastman Chemical Company

    Category Notes
    Plastic

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

     

    Proto3000 – 3D Engineering Solutions
    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.