MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Zircar Refractory Composites RS-1200 Refractory Sheet
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: ZIRCAR Refractory Sheet Type RS-1200 is a high strength composite designed for use as thermo-mechanical and electrical insulation in applications with temperatures as high as 1300°C(2372°F). RS-1200 is a combination of strong reinforcing fibers tightly bound in an alumina ceramic matrix. RS-1200 is completely inorganic and contains no asbestos or RCF fibers. RS-1200 exhibits greater refractoriness and homogeneity than other reinforced alumina matrix composite products and can be readily machined to tight tolerances with conventional carbide tooling.

Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)

Vendors:
Available Properties
  • Density
  • Loss On Ignition
  • Porosity
  • Hardness, Shore D
  • Modulus of Rupture, parallel to thickness
  • Compressive Yield Strength, at 2% compression parallel to thickness
  • Volume Resistivity
  • Surface Resistance
  • Dielectric Strength
  • Dielectric Breakdown, 1/8 in. thick
  • Arc Resistance
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity, parallel to thickness
  • Thermal Conductivity, parallel to thickness
  • Thermal Conductivity, parallel to thickness
  • Thermal Conductivity, parallel to thickness
  • Melting Point
  • Maximum Service Temperature, Air
  • Flammability Test, Nil
  • Shrinkage, perpendicular to thickness
  • Shrinkage, perpendicular to thickness
  • Al2O3
  • Other
  • SiO2
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Zircar Refractory Composites, Inc.

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.