MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Rogers Corporation RO3210 Woven-Glass Reinforced PTFE Laminate
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Glass Filled, Molded

Material Notes: Features and Benefits:
  • Woven glass reinforcement - Improves rigidity for easier handling
  • Uniform electrical and mechanical performance - ideal for complex multi-layer high frequency structures
  • Low dielectric loss - high frequency performance can be used in applications exceeding 20 GHz
  • Low in-plane expansion coefficient (match to copper) - suitable for use with epoxy multi-layer board hybrid designs and allows for more reliable surface mounted assemblies
  • Excellent dimensional stability - high production yields
  • Economically priced - cost effective volume manufacturing
  • Surface smoothness- allows for finer line etching tolerances
  • Lead-free process compatible

Uses:

  • Automotive collision avoidance systems
  • Automotive global positions satellite antennas
  • Wireless telecommunications systems
  • Microstrip patch antennas for wireless communications
  • Direct broadcast satellites
  • Datalink on cable systems
  • Remote meter readers
  • Power backplanes
  • LMDS and wireless broadband
  • Base station infrastructure

Information provided by Rogers Corporation.

Vendors:
Available Properties
  • Density
  • Water Absorption, IPC-TM-2.4.8, D24/23
  • Thickness, Range of Thicknesses Available
  • Tensile Modulus, ASTM D638, TD
  • Tensile Modulus, ASTM D638, MD
  • Peel Strength, IPC-TM-650 2.4.8, Copper; 1 oz. EDC After Solder Float
  • Volume Resistivity, IPC 2.5.17.1, Cond. A
  • Surface Resistance, IPC 2.5.17.1, Cond. A
  • Dielectric Constant, IPC-TM-650 2.5.5.5, Clamped stripline, Z-direction
  • Dielectric Constant, Differential Phase Length Method, Z-Direction
  • Dissipation Factor, IPC-TM-650 2.5.5.5
  • CTE, linear, ASTM D3386-94, X, Y- Direction
  • CTE, linear, ASTM D3386-94, Z-Direction
  • Specific Heat Capacity, Calculated
  • Thermal Conductivity, ASTM C518
  • Decomposition Temperature, ASTM D3850, TGA
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.