MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
3M Dyneon™ PFA 6502TZ Perfluoroalkoxy Fluorothermoplastic Granules
Categories: Polymer; Thermoplastic; Fluoropolymer; Perfluoroalkoxy (PFA)

Material Notes: 3M™ Dyneon™ PFA 6502TZ is a fluorothermoplastic resin for transfer molding applications and extrusion of claddings and linings. Dyneon PFA 6502TZ allows for easy processing under low shear rates, with a wide processing window and excellent color stability. This material can be used in tough environments, such as chemical industry applications, where high strength and extreme thermal and chemical resistance are required.

Features and Benefits:

  • Wide service temperature range
  • Excellent, almost universal resistance to solvents and chemicals
  • High transparency
  • Extremely high weathering resistance and UV stability
  • Smooth surfaces
  • Broad processing window
  • High limiting oxygen index: does not support combustion
  • Good non stick characteristics
  • Excellent electrical insulation properties
  • Excellent mold release
  • Good low friction properties
  • Excellent stress crack resistance
  • Transfer molding and extrusion
Information provided by Dyneon, A 3M Company

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Melt Index of Compound, ASTM D1238
  • Hardness, Shore D, ASTM D2240
  • Tensile Strength at Break, ASTM D638
  • Elongation at Break, ASTM D638
  • Flexural Modulus, ASTM D790
  • Melting Point, ASTM D4591
  • Oxygen Index, ASTM D2863
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Dyneon, Division of 3M

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.