MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Extreme Materials from MCAM
Visit Mitsubishi Chemical Advanced Materials for Extreme Materials - high performance plastic machining stock engineered to replace metals such as nickel alloys or stainless steel.
Haynes 625SQ® Nickel Alloy Sheet
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: Haynes 625SQ alloy is a solid-solution strengthened superalloy. It is a modification of Haynes 625 alloy designed to enhance resistance to fatigue at temperatures up to approximately 1200°F (649°C). The alloy composition is tightly controlled to very low levels of carbon, silicon, and nitrogen. Primary melting is by vacuum induction melting, followed by consumable electrode practice using electroslag remelting. During processing, the grain size is controlled to ASTM #5 or finer. Haynes 625SQ alloy sheet and strip meet the requirements of AMS 5879 and AMS 5599 specifications. Haynes 625SQ alloy is readily fabricated and welded using practices common to Haynes 625 alloy. Haynes 625SQ alloy sheet and strip find application in aerospace, automotive, and chemical process industry bellows, expansion joints, and fabrications where fatigue resistance, strength, and corrosion resistance are required.

Data provided by the manufacturer, Haynes International, Inc.

Vendors:
Available Properties
  • Density
  • Tensile Strength, Ultimate, AMS 5879
  • Tensile Strength, Ultimate, AMS 5879
  • Tensile Strength, Ultimate, AMS 5879
  • Tensile Strength, Ultimate, AMS 5879
  • Tensile Strength, Ultimate, AMS 5879
  • Tensile Strength, Ultimate, AMS 5879
  • Tensile Strength, Ultimate, AMS 5879
  • Tensile Strength, Yield, AMS 5879
  • Tensile Strength, Yield, AMS 5879
  • Tensile Strength, Yield, AMS 5879
  • Tensile Strength, Yield, AMS 5879
  • Tensile Strength, Yield, AMS 5879
  • Tensile Strength, Yield, AMS 5879
  • Tensile Strength, Yield, AMS 5879
  • Elongation at Break, AMS 5879, 2-inch (51 mm) sample
  • Elongation at Break, AMS 5879, 2-inch (51 mm) sample
  • Elongation at Break, AMS 5879, 2-inch (51 mm) sample
  • Elongation at Break, AMS 5879, 2-inch (51 mm) sample
  • Elongation at Break, AMS 5879, 2-inch (51 mm) sample
  • Elongation at Break, AMS 5879, 2-inch (51 mm) sample
  • Elongation at Break, AMS 5879, 2-inch (51 mm) sample
  • Modulus of Elasticity, Dynamic
  • Modulus of Elasticity, Dynamic
  • Modulus of Elasticity, Dynamic
  • Modulus of Elasticity, Dynamic
  • Modulus of Elasticity, Dynamic
  • Modulus of Elasticity, Dynamic
  • Modulus of Elasticity, Dynamic
  • Modulus of Elasticity, Dynamic
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  • Annealing Temperature, AMS 5879, Bright Anneal
  • Aluminum, Al
  • Carbon, C
  • Cb + Ta
  • Chromium, Cr
  • Cobalt, Co
  • Iron, Fe
  • Manganese, Mn
  • Molybdenum, Mo
  • Nickel, Ni, as balance
  • Nitrogen, N
  • Silicon, Si
  • Titanium, Ti
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Haynes International, Inc.

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Master Bond adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.