MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Eastman Optifilm™ 400 Enhancer
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Description: Eastman Optifilm™ enhancer 400 is a low odor coalescent that is compatible with a variety of latex types and it does not contribute to the VOC content of paints. It is an efficient coalescent that aids in the development of latex paints that have a good balance of performance properties. Optifilm 400 delivers excellent film integrity, touch-up properties, and scrub resistance, even at the lowest VOCs content. Paints prepared with Optifilm 400 have also demonstrated good exterior durability after one year exposure. It can also be blended with other coalescents such as Eastman Texanol™ ester alcohol or Eastman EEH glycol ether to further optimize the balance of low VOC content and paint performance. Optifilm 400 is compatible with solvent borne acrylic resins and improves the flexibility and adhesion of coatings based on these resins. This product is non-phthalate and is not listed as a HAP or on SARA 313.

Application/Uses:

  • Coatings - Architectural
  • Coatings - Can and Coil
  • Coatings - General Industrial
  • Coatings - Industrial Maintenance and Marine
  • Coatings - Industrial Wood
Key Attributes:
  • Extremely low odor
  • Good coalescing efficiency
  • Non-HAP
  • Non-SARA
  • Non-yellowing
  • REACH compliant
  • Readily biodegradable
  • Stable in low to high pH coatings
  • Zero VOC contribution to paint

Information provided by Eastman

Vendors:
Available Properties
  • Density
  • Viscosity
  • Vapor Pressure
  • Melting Point, Freezing Point
  • Boiling Point, @ 760 mm Hg
  • Flash Point, ensky-Martens Closed Cup
  • Refractive Index
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Eastman Chemical Company

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.