MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
High Strength Modified Copper, UNS C19400, H04 Temper flat products
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent hot and cold workability.

Applications: circuit breaker components, contact springs, electrical clamps, electrical springs, electrical terminals, flexible hose, fuse clips, gaskets, gift hollow ware, plug contacts, rivets, and welded condenser tubes.

Test specimen: flat product - 1mm thickness.

Key Words: CDA 194, HSM Copper
Vendors:
Available Properties
  • Density
  • Hardness, Rockwell B
  • Hardness, Rockwell 30T
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate, annealed strip
  • Tensile Strength, Ultimate, annealed strip
  • Tensile Strength, Ultimate, annealed strip
  • Tensile Strength, Ultimate, annealed strip
  • Tensile Strength, Ultimate, annealed strip
  • Tensile Strength, Ultimate, annealed strip
  • Tensile Strength, Ultimate, annealed strip
  • Tensile Strength, Ultimate, annealed strip
  • Tensile Strength, Ultimate, annealed strip
  • Tensile Strength, Ultimate, annealed strip
  • Tensile Strength, Ultimate, annealed strip
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate, annealing response of strip
  • Tensile Strength, Ultimate, annealing response of strip
  • Tensile Strength, Ultimate, annealing response of strip
  • Tensile Strength, Ultimate, annealing response of strip
  • Tensile Strength, Ultimate, annealing response of strip
  • Tensile Strength, Ultimate, annealing response of strip
  • Tensile Strength, Ultimate, annealing response of strip
  • Tensile Strength, Ultimate, annealing response of strip
  • Tensile Strength, Ultimate, annealing response of strip
  • Tensile Strength, Ultimate, annealing response of strip
  • Tensile Strength, Ultimate, annealing response of strip
  • Tensile Strength, Ultimate, annealing response of strip
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield, annealed strip
  • Tensile Strength, Yield, annealed strip
  • Tensile Strength, Yield, annealed strip
  • Tensile Strength, Yield, annealed strip
  • Tensile Strength, Yield, annealed strip
  • Tensile Strength, Yield, annealed strip
  • Tensile Strength, Yield, annealed strip
  • Tensile Strength, Yield, annealed strip
  • Tensile Strength, Yield, annealed strip
  • Tensile Strength, Yield, annealed strip
  • Tensile Strength, Yield, annealed strip
  • Tensile Strength, Yield, annealing response of strip
  • Tensile Strength, Yield, annealing response of strip
  • Tensile Strength, Yield, annealing response of strip
  • Tensile Strength, Yield, annealing response of strip
  • Tensile Strength, Yield, annealing response of strip
  • Tensile Strength, Yield, annealing response of strip
  • Tensile Strength, Yield, annealing response of strip
  • Tensile Strength, Yield, annealing response of strip
  • Tensile Strength, Yield, annealing response of strip
  • Tensile Strength, Yield, annealing response of strip
  • Tensile Strength, Yield, annealing response of strip
  • Tensile Strength, Yield, annealing response of strip
  • Elongation at Break, In 50 mm
  • Elongation at Break
  • Elongation at Break, annealing response of strip
  • Elongation at Break, annealing response of strip
  • Elongation at Break, annealing response of strip
  • Elongation at Break, annealing response of strip
  • Elongation at Break, annealing response of strip
  • Elongation at Break, annealing response of strip
  • Elongation at Break, annealing response of strip
  • Elongation at Break, annealing response of strip
  • Elongation at Break, annealing response of strip
  • Elongation at Break, annealing response of strip
  • Elongation at Break, annealing response of strip
  • Elongation at Break, annealing response of strip
  • Creep Strength, annealed strip
  • Creep Strength, annealed strip
  • Creep Strength, annealed strip
  • Creep Strength, annealed strip
  • Creep Strength, annealed strip
  • Creep Strength, annealed strip
  • Creep Strength, annealed strip
  • Creep Strength, annealed strip
  • Rupture Strength, annealed strip
  • Rupture Strength, annealed strip
  • Rupture Strength, annealed strip
  • Rupture Strength, annealed strip
  • Rupture Strength, annealed strip
  • Rupture Strength, annealed strip
  • Rupture Strength, annealed strip
  • Modulus of Elasticity
  • Poissons Ratio
  • Fatigue Strength, rotating beam test
  • Machinability, UNS C36000 (free-cutting brass) = 100%
  • Forgeability
  • Shear Modulus
  • Electrical Resistivity
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  • Annealing Point
  • Copper, Cu
  • Iron, Fe
  • Lead, Pb
  • Other, total
  • Phosphorus, P
  • Tin, Sn
  • Zinc, Zn
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.