MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Extreme Materials from MCAM
Visit Mitsubishi Chemical Advanced Materials for Extreme Materials - high performance plastic machining stock engineered to replace metals such as nickel alloys or stainless steel.
Special Metals INCONEL® Alloy 718
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Developed in the early 1960's, IN718 is still considered the material of choice for the majority of aircraft engine components with service temperatures below 1200°F (650°C). Inconel 718 is a precipitation-hardenable nickel-chromium alloy containing also significant amounts of iron, niobium, and molybdenum along with lesser amounts of aluminum and titanium. It combines corrosion resistance and high strength with outstanding weldability including resistance to postweld cracking. The alloy has excellent creep-rupture strength at temperatures to 1300°F (700°C).

Applications: Aerospace, gas turbines, rocket motors, spacecraft, space shuttles, nuclear reactors, pumps, turbo pump seals, and tooling.

Forms: round, flat, extruded section, pipe, tube, forging stock, plate, sheet, strip and wire.

Data provided by the manufacturer, Special Metals.

Key Words: IN718, INCONEL 718, AFNOR NC 19 Fe Nb, UNS N07718; ASTM B637, B670; ASME Boiler Code Sections I, III; AMS 5589, AMS 5590, AMS 5596, AMS 5597, AMS 5662, AMS 5663, AMS 5664, AMS 5832, Werkstoff Nr. 2.4668; WL Nr. 2.4668; MIL-N-24469; NACE MR-01-75; AECMA Pr EN 2404, 2405, 2407, 2408, 2952, 2961, 3219
Vendors:
Available Properties
  • Density
  • Tensile Strength, Ultimate, Precipitation Hardened prior to test
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield, Precipitation Hardened. Value at room temperature
  • Tensile Strength, Yield, Precipitation Hardened prior to test
  • Elongation at Break, Precipitation Hardened
  • Elongation at Break, Precipitation Hardened prior to test.
  • Rupture Strength
  • Rupture Strength
  • Electrical Resistivity
  • Magnetic Permeability, at 200 Oersted (15.9 kA/m)
  • Curie Temperature
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  • Aluminum, Al
  • Boron, B
  • Carbon, C
  • Chromium, Cr
  • Cobalt, Co
  • Copper, Cu
  • Iron, Fe, As remainder
  • Manganese, Mn
  • Molybdenum, Mo
  • Nickel, Ni, includes cobalt
  • Niobium, Nb (Columbium, Cb)
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  • Titanium, Ti
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Special Metals (includes the former Inco Alloys International Inc.)

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.