MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Carpenter Thermo-Span® Fe-Co-Ni Superalloy
Categories: Metal; Superalloy; Iron Base

Material Notes: Data provided by Carpenter Technology Corporation.

Thermo-Span® alloy is a precipitation hardenable superalloy which exhibits a low coefficient of thermal expansion over a broad temperature range, high tensile and rupture strengths, and good thermal fatigue resistance. This alloy offers a significant improvement in environmental resistance over Pyromet® alloys CTX-1, CTX-3, AND CTX-909 due to the addition of chromium. the alloy also possesses an excellent combination of tensile properties and stress rupture strength in the recrystallized condition with the use of common solution and age hardening treatments. Unlike the CTX-family of alloys, the use of specific braze-cycle age hardening treatments is not required for Thermo-Span alloy due to the higher solution treating temperature.

Thermo-Span alloy should be considered for use in all applications for which the current low expansion superalloys are suited. These include compressor and exhaust casings, seals and other gas turbine components. Additional high temperature applications where moderate oxidation resistance is required are feasible with Thermo-Span alloy. This alloy should also be considered for use in applications requiring resistance to thermal fatigue.

Thermo-Span® is a registered trademark of Carpenter Technology Corporation.

Vendors:
Available Properties
  • Density
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Elongation at Break, In 4D
  • Elongation at Break, In 4D
  • Elongation at Break, In 4D
  • Elongation at Break, In 4D
  • Elongation at Break, In 4D
  • Elongation at Break, In 4D
  • Elongation at Break, In 4D
  • Elongation at Break, In 4D
  • Reduction of Area
  • Reduction of Area
  • Reduction of Area
  • Reduction of Area
  • Reduction of Area
  • Reduction of Area
  • Reduction of Area
  • Reduction of Area
  • Modulus of Elasticity
  • Modulus of Elasticity
  • Modulus of Elasticity
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Aluminum, Al
  • Boron, B
  • Carbon, C
  • Chromium, Cr
  • Cobalt, Co
  • Copper, Cu
  • Iron, Fe, as remainder
  • Manganese, Mn
  • Nickel, Ni
  • Niobium, Nb (Columbium, Cb)
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  • Titanium, Ti
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Carpenter Technology Corporation (Cartech)

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.