MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
LyondellBasell BMC T60-6009 Compression Grade Wear Resistant Molding Compound
Categories: Polymer; Thermoset; Polyester, TS; Polyester (Thermoset) - Rigid

Material Notes: BMC T60-6009 is a compression grade wear resistant molding compound. This material was specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cost per cubic inch savings. BMC T60-6009 is UL listed and is typically used in power distribution equipment, switching components/relays, constant use switch applications and circuit protection breakers.

Information provided by Bulk Molding Compounds, Inc.

LyondellBasell has acquired A. Schulman, Inc..

Vendors:
Available Properties
  • Specific Gravity
  • Density, Molded
  • Linear Mold Shrinkage
  • Linear Mold Shrinkage
  • Hardness, Barcol
  • Tensile Strength
  • Tensile Strength
  • Flexural Strength
  • Flexural Strength
  • Flexural Modulus
  • Flexural Modulus
  • Compressive Strength
  • Compressive Strength
  • Izod Impact, Notched
  • Izod Impact, Notched (ISO)
  • Dielectric Strength
  • Dielectric Strength, short time
  • Arc Resistance
  • Arc Resistance
  • Comparative Tracking Index
  • Comparative Tracking Index
  • Maximum Service Temperature, Air, RTI
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Flammability, UL94
  • Flammability, UL94, Black
  • Flammability, UL94, All Colors
  • Processing Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
LyondellBasell, A. Schulman, former BMC - Bulk Molding Compounds Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.