  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
EDRO EDRO400™ #40 Prehardened Insert Quality Martensitic Stainless Steel
Categories: Metal; Ferrous Metal; Martensitic; Stainless Steel; T 400 Series Stainless Steel

Material Notes: EDRO400™ is a remelted 400 series martensitic stainless steel supplied prehardened to 40 HRC (375 HB).
EDRO400™ is characterized by excellent polishability, superior corrosion resistance, high level of dimensional stability, enhanced machinability, good ductility and toughness, uniform and consistent hardness, good thermal conductivity, good resistance to indentation (compressive strength), smooth as rolled plate surfaces, and excellent weldability.
EDRO400™ chemical composition, melting and refining practice and thermal treatment establish physical and mechanical properties designed to provide homogeneity, superior polished surface finishes, improved corrosion resistance, reduced mold maintenance costs, dimensional stability, uniform and consistent hardness, and safe and simple weld repair.
Applications: plastic injection mold inserts / cavities, extrusion tooling, rubber molds, components, and constructional parts

Information provided by EDRO

Key Words: 420 ESR
Vendors:
Available Properties
  • Density
  • Density
  • Hardness, Rockwell C
  • Hardness, Vickers, Gas Nitriding, thickness refers to distance from surface
  • Hardness, Vickers, Gas Nitriding, thickness refers to distance from surface
  • Hardness, Vickers, Plasma Nitriding, thickness refers to distance from surface
  • Hardness, Vickers, Plasma Nitriding, thickness refers to distance from surface
  • Hardness, Vickers, Plasma Nitriding, thickness refers to distance from surface
  • Hardness, Vickers, Gas Nitriding, thickness refers to distance from surface
  • Hardness, Vickers, Gas Nitriding, thickness refers to distance from surface
  • Hardness, Vickers, Plasma Nitriding, thickness refers to distance from surface
  • Hardness, Vickers, Gas Nitriding, thickness refers to distance from surface
  • Hardness, Vickers, Gas Nitriding, thickness refers to distance from surface
  • Hardness, Vickers, Plasma Nitriding, thickness refers to distance from surface
  • Tensile Strength, Ultimate, Longitudinal Tests from 6.3" rolled plate at 375 HB
  • Tensile Strength, Yield, Longitudinal Tests from 6.3" rolled plate at 375 HB
  • Elongation at Yield, in 2"
  • Reduction of Area
  • Modulus of Elasticity
  • Modulus of Elasticity
  • Charpy Impact, Average CharpyV-notch from 6.3" plate at 387 HB
  • CTE, linear
  • Thermal Conductivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.