MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
CHT Group QSil 220 Transparent, Liquid Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: Product Description: QSil 220 is a two-part, clear, liquid silicone which cures at elevated temperatures. It has a low viscosity which allows for ease of flow around complex parts, providing electrical insulation and shock resistance. The chemical composition provides hydrolytic and reversion resistance. This material also has excellent, primerless adhesion to most substrates.

Key Features:

  • Convenient 10:1 mixing ratio for use in automatic dispensing equipment or hand mixing
  • Contains no solvents
  • Non-yellowing catalyst system
  • Heat cure required to obtain full properties and adhesion

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors:
Available Properties
  • Specific Gravity, Uncatalyzed, QSil 220B
  • Specific Gravity, Uncatalyzed, QSil 220A
  • Viscosity, Uncatalyzed, QSil 220B
  • Viscosity, Uncatalyzed, QSil 220A
  • Linear Mold Shrinkage, Cured 60 minutes @ 100°C
  • Hardness, Shore A, Cured 60 minutes @ 100°C
  • Tensile Strength, Cured 60 minutes @ 100°C
  • Elongation at Break, Cured 60 minutes @ 100°C
  • Tensile Modulus, Young's, Cured 60 minutes @ 100°C
  • CTE, linear
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Flammability, UL94
  • Refractive Index, Cured 60 minutes @ 100°C
  • Cure Time
  • Cure Time
  • Cure Time
  • Gel Time, Catalyzed
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.