MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Daikin ZEFFLE SE-405 Fluoro Resin
Categories: Polymer; Thermoplastic; Fluoropolymer

Material Notes: ZEFFLE SE is a weatherable fluoro resin for paint. Its emulsion base resin could reduce VOC of your formulation. SE-405 is excellent in low temperature film forming.

Introduction: ZEFFLE SE-405 is an emulsion resin consisting of VdF-copolymer and acrylic polymer; Excellent weather resistance, and initial water resistance; Best fit with paint targeted on concrete or water proof sheet as the resin is flexible to substrate; Film can be formed by lower temperature; It can be formulated into onsite paint as well as industrial paint; No solvent odor and no worry of inflammability; SE-405 is an elastic type and can be used for paints used elastic substrates

Information provided by Daikin.

Vendors:
Available Properties
  • Solids Content, Dried by 170? for 30 minutes
  • Particle Size, Average
  • pH
  • Minimum Service Temperature, Air, MFT
  • Glass Transition Temp, Tg
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Daikin Industries

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.