MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
ChevronTexaco Cleartex® E
Categories: Fluid; Lubricant

Material Notes: Texaco Cleartex metalworking fluids deliver value through:
  • Multipurpose performance — Texaco Cleartex cutting oils are tri-purpose, serving as the cutting oil, hydraulic fluid and machine lubricant in machine tools to eliminate the problem of machine lubricants contaminating the cutting oil.
  • Transparent, light color allows operator to better see the machined part during the cutting operation.
  • Excellent EP properties provide extended tool life and improved surface finish while protecting against staining of yellow metals.
  • Antimist control minimizes the amount of stray mist around the machine, improving shop cleanliness and reducing operator exposure.

Texaco Cleartex cutting oils are transparent, light colored, chlorinated cutting oils. The EP compounding in Texaco Cleartex cutting oils is nonstaining to yellow metals, provides long tool life and allows for faster machine rates.

Texaco Cleartex cutting oils can be used as the cutting oil, hydraulic oil and machine lubricant in automatic screw machines. This eliminates the contamination problem caused by leakage of these fluids into the cutting oil, reducing cutting oil effectiveness. Texaco Cleartex cutting oils are effective at providing rust and corrosion protection of parts, cutting tools and the machine.

Texaco Cleartex cutting oils are formulated with paraffinic base stocks with a naturally high viscosity index. These cutting oils have high flash points, minimizing the potential for fire.

They also contain an effective mist control agent that reduces stray mist around the machine. This improves shop cleanliness and reduces operator exposure to the cutting oil.

Texaco Cleartex metalworking fluids:

  • provide excellent cooling and lubrication in a wide range of machining operations
  • prevent welding of chip and tool
  • flush chips away from the work area
  • protect the finished work surfaces, tools and
  • machines against rusting and staining
  • reduce oil mist in high speed machine tools

Texaco Cleartex D and E are intended for use as general purpose cutting oils where the machining requirements range from light to moderately severe. They are recommended for the machining operations on free-machining to intermediate steels and difficult to machine nonferrous metals. Texaco Cleartex E is also recommended where a higher viscosity product would be preferred for the machining or hydraulic application.

Texaco Cleartex cutting oils are widely used in automatic screw machines and NC/CNC machining centers. The tri-purpose nature of Texaco Cleartex cutting oils allows the user to minimize inventories of other fluids.

Do not use Texaco Cleartex cutting oils in high pressure systems in the vicinity of flames, sparks and hot surfaces. Use only in well ventilated areas. Keep container closed.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

CPS Number: 222237; MSDS Number: 8905

Vendors:
Available Properties
  • API Gravity
  • Viscosity Measurement, Viscosity Index
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • ASTM Color, L
  • Flash Point
  • Transmission, Visible, clear; thickness not quantified
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
ChevronTexaco Corp

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.