MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Covestro Makroblend® DP UT3905 Polycarbonate + PBT, Impact Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes:
  • Developmental product
  • (PC+PBT)-blend
  • high flow
  • impact modified
  • easy release
  • injection molding grade
Makroblend DP UT3905* offers superior flowability, good impact strength and excellent chemical resistance.

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors:
Available Properties
  • Density, ISO 1183
  • Melt Density
  • Water Absorption, Similar to ISO 62
  • Moisture Absorption at Equilibrium, Similar to ISO 62
  • Melt Flow, ISO 1133
  • Tensile Strength, Yield, ISO 527-1/-2
  • Elongation at Break, ISO 527-1/-2, Nominal
  • Elongation at Yield, ISO 527-1/-2
  • Tensile Modulus, ISO 527-1/-2
  • Charpy Impact Unnotched, ISO 179/1eU
  • Charpy Impact Unnotched, ISO 179/1eU
  • Charpy Impact, Notched, ISO 179/1eA
  • Charpy Impact, Notched, ISO 179/1eA
  • Impact, ISO 6603-2, Puncture - maximum force (N)
  • Impact, ISO 6603-2, Puncture - maximum force (N)
  • Puncture Energy, ISO 6603-2
  • Puncture Energy, ISO 6603-2
  • Volume Resistivity, IEC 60093
  • Surface Resistance, IEC 60093
  • Dielectric Constant, IEC 60250
  • Dielectric Constant, IEC 60250
  • Dielectric Strength, IEC 60243-1
  • Dissipation Factor, IEC 60250
  • Dissipation Factor, IEC 60250
  • Comparative Tracking Index, IEC 60112
  • CTE, linear, Parallel to Flow, ISO 11359-1/-2
  • CTE, linear, Transverse to Flow, ISO 11359-1/-2
  • Specific Heat Capacity, Melt
  • Thermal Conductivity, Melt
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75-1/-2
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-1/-2
  • Flammability, UL94, IEC 60695-11-10
  • Oxygen Index, ISO 4589-1/-2
  • Melt Temperature
  • Melt Temperature, ISO 294, Injection Molding
  • Mold Temperature
  • Mold Temperature, ISO 10724, Injection Molding
  • Mold Temperature
  • Ejection Temperature
  • Injection Velocity, ISO 294
  • Drying Temperature
  • Dry Time, Dry air dryer
  • Dry Time, Fresh air dryer (high speed dryer)
  • Dry Time, Circulating air drying oven (50 % fresh air)
  • Moisture Content
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Covestro Deutschland AG, Bayer MaterialScience

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.