MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Schmolz + Bickenbach UGIMA® 303 Stainless Steel Bar
Categories: Metal; Ferrous Metal; Stainless Steel; T 300 Series Stainless Steel

Material Notes: 303 UGIMA® is Ugitech’s improved machining grade produced only by Ugitech. It is identical in every way to regular 303, except with respect to machinability. 303 UGIMA® represents Ugitech's popular UGIMA® family of high machinability grades. Through the use of new and beneficial modifications to the steel-making process, 303 UGIMA® builds upon the proprietary UGIMA® manufacturing process to allow for excellent machinability across a wider range of operations and cutting conditions. When compared with older versions, 303 UGIMA® is a technologically advanced product that will allow for superior machinability at both low and high speeds, in cam-driven and CNC machines, and with high-speed steel or carbide tooling. Machine shops using 303 UGIMA® have experienced consistent success regardless of machine, operation, tooling, or cutting conditions. From lot to lot, 303 UGIMA® is engineered to give the same high performance every time without surprises.

Applications: Fasteners, Shafts, Valve Bodies, Valves, Valve Trim, Fittings, Machined parts, and Not recommended for vessels containing liquid or gasses at high pressures

Information provided by Schmolz + Bickenbach

Key Words: AISI 303; UNS S30300; EN 10088-3 1.4305; X8CrNiS 18-8; SAE J405; ASTM A314; ASTM A320 Class 1; A484; A581; A582; F899; AMS 5640 Type 1; QQ-S-763C; QQ-S_764B, Amend 2; MIL-S-862; MIL-W-52263C
Vendors:
Available Properties
  • Density
  • Hardness, Brinell, Escomatic Coils
  • Hardness, Brinell, Turned Bars
  • Hardness, Brinell, Cold Drawn Bars
  • Tensile Strength, Escomatic Coils
  • Tensile Strength, Turned Bars
  • Tensile Strength, Cold Drawn Bars
  • Tensile Strength, Yield, Escomatic Coils
  • Tensile Strength, Yield, Turned Bars
  • Tensile Strength, Yield, Cold Drawn Bars
  • Elongation at Yield, Escomatic Coils
  • Elongation at Yield, Cold Drawn Bars
  • Elongation at Yield, Turned Bars
  • Reduction of Area, Escomatic Coils
  • Reduction of Area, Cold Drawn Bars
  • Reduction of Area, Turned Bars
  • Electrical Resistivity
  • CTE, linear
  • Thermal Conductivity
  • Annealing Temperature, Followed by rapid cooling with forced air or water quenching
  • Hot-Working Temperature, Forging range
  • Hot-Working Temperature, Heat in range
  • Carbon, C
  • Chromium, Cr
  • Copper, Cu
  • Iron, Fe
  • Manganese, Mn
  • Molybdenum, Mo
  • Nickel, Ni
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Schmolz + Bickenbach (Swiss Steel International)

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.