MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Chemically Resistant adhesives
Master Bond EP42HT-3AO Two part, room temperature curable epoxy system
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive; Epoxy Encapsulant, Unreinforced

Material Notes: Key Features:
  • Convenient handling, long working life
  • Thermal conductive and electrical insulative
  • High glass transition temperature
  • Low coefficient of thermal expansion
Master Bond EP42HT-3AO is thermally conductive, electrically insulating epoxy for bonding, sealing, coating and encapsulation applications. It is relatively easy to use with a forgiving 100 to 40 mix ratio by weight. It will cure in 3-4 days at room temperature or 2-3 hours at 150-200°F. To optimize properties, the recommended curing is overnight at room temperature followed by 2-3 hours at 150-200°F. Upon mixing, EP42HT-3AO is a moderate viscosity system with very good flow properties. Among its many favorable attributes, this system has a high glass transition temperature and a low coefficient of thermal expansion. It bonds well to a wide variety of substrates including metals, composites, ceramics, glass and many plastics. Some positives include its low shrinkage upon curing and stellar dimensional stability. It is resistant to water, oils, acid, bases and many solvents. The service temperature range is from -100°F to +400°F. The color of Part A is white and the color of Part B is off-white. This blend of product properties allows this distinctive formulation to be used in specialty electronic, optical, opto-electronic, aerospace and related industries.

Product Advantages:

  • Forgiving 100:40 mix ratio by weight
  • Good flow, long working life
  • Cures at ambient and elevated temperatures
  • Superior thermal and dimensional stability
  • Very good thermal conductivity and electrical insulation
  • Combines low CTE and high Tg
  • Meets NASA low outgassing specification

Information provided by Masterbond.

Vendors:
Available Properties
  • Viscosity, Part B
  • Viscosity, mixed
  • Viscosity, Part A
  • Hardness, Shore D
  • Tensile Strength
  • Elongation at Break
  • Tensile Modulus
  • Adhesive Bond Strength, lap shear, Al/Al
  • Volume Resistivity
  • Dielectric Constant
  • CTE, linear
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Glass Transition Temp, Tg
  • Cure Time
  • Cure Time
  • Working Life, After mixing, 100 g batch
  • Shelf Life, In original unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.