MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
Lanxess LEWATIT® MonoPlus MK 51 Anion Exchange Resin
Categories: Polymer; Thermoset

Material Notes: Lewatit® MonoPlus MK 51 is a styrene-based, monodispersed, macroporous weak base anion exchanger with polyhydroxy groups showing a very high selectivity for the removal of boric acid or borates from water. The high selectivity of borate to the resin allows a separation of boric acid from water and aqueous electrolyte solutions also a high salt concentration. Lewatit MonoPlus MK 51 can especially be used for:
  • the removal of boron from waste water or contaminated ground water
  • the removal of boron from RO permeate in purpose to produce water for irrigation
  • the removal of boron traces in the production of ultrapure water or chemicals
  • removal of boron from high concentrated magnesium chloride solution
  • adsorption of oxoanions of W, Mo, V Ge, As, Sb, from processes streams
The resin is appropriately exhausted at a specific flow rate of 10…20 BV/h. The regeneration can be done with hydrochloric or sulfuric acid. To reach high capacity levels it is recommended to make a two stage regeneration using a sodium hydroxide solution for the second treatment (conditioning).

Information provided by Lanxess.

Vendors:
Available Properties
  • Bulk Density
  • Density
  • Bead Size, Mean
  • Storage Temperature
  • Maximum Service Temperature, Air
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Lanxess, Spinoff of Bayer

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Master Bond adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.