| MPP-D45B is polyether based polyurethane casting resin formulation for a variety of custom applications. The cured material has a good physical strength for this class of material with hardness of 95A to 45D Durometer for a good load bearing capacity with flexibility. The component materials are liquid at room temperature and can be processed without use of auxiliary heating in low-cost molds. Relatively low viscosity of raw material components allows easy mix and good mold resolution. This set of properties makes MPP-D45B an excellent choice for making aftermarket bushings, impact pads, prototyping, short-run productions, and many other applications. MPP-D45B Part-A Component: MPB-025 Part-B Component: PBB-016 Mixing Ratio: 100: 75 = Part-A: Part-B by Weight (100: 82 by Volume) Information provided by Northstar Polymers |