| MPP-D73C is formulated to meet requirements of molding custom parts by either manual hand-mixing/casting or by meter mixing dispensers. The cured material is rigid enough for some load bearing parts, yet it has some flexibility to resist cracking from impact force. All process can be done at room temperature. The low viscosity components make it easy to mix, degas, and cast. The reasonably long pot-life and quick demolding time contributes to higher production rate with easier casting process. The mixing ratio is easy 1:2 by volume, which is convenient metering. Part-A Component: MNA-014 Part-B Component: PNC-025 Mixing Ratio: 1: 2 by volume (1: 1.685 by weight) = part-A: part-B Information provided by Northstar Polymers |