MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Ovako 18CrNiMo7-6 159Q Steel, Hardening
Categories: Metal; Ferrous Metal; Alloy Steel; AISI 4000 Series Steel

Material Notes: General Information: 18CrNiMo7-6 is a case hardening steel with high toughness. There are a number of variants with high cleanliness requirements. All variants possess tighter composition ranges compared to the standard. One variant is produced with the quality class IQ (isotropic quality). This ensures a very low number of elongated sulphide inclusions which will give more isotropic properties. The high oxidic cleanliness will enable the steel to meet the same high cleanliness demands as for re-melted qualities.
Grade 159A - Variant with low sulphur content and high cleanliness demands
Grade 159B - Variant with controlled sulphur content for consistent machinability and +H hardenability
Grade 159Q - Isotropic properties (IQ) and better fatigue strength due to higher cleanliness levels, and a finer size and distribution of non-metallic inclusions
Grade 159X - Variant with controlled sulphur content for consistent machinability and +H hardenability
Grade 159S - Variant with increased sulphur content.
Grade 4761(MoCN216) - Low sulphur variant of ImatraIQ-SteelIQ-SteelĀ® is an isotropic quality ultra clean steel optimized for high fatigue strength under multi axial loading.

Information provided by Ovako

Key Words: 1.6587, AISI4820, DIN17CrNiMo6, 18CND6
Vendors:
Available Properties
  • Density
  • Tensile Strength
  • Tensile Strength
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Elongation at Break
  • Elongation at Break
  • Modulus of Elasticity
  • Poissons Ratio
  • Shear Modulus
  • Electrical Resistivity
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity, Ambient temperature
  • Transformation Temperature, MS
  • Transformation Temperature, AC1
  • Transformation Temperature, AC3
  • Carbon, C
  • Chromium, Cr
  • Iron, Fe, As Balance
  • Manganese, Mn
  • Molybdenum, Mo
  • Nickel, Ni
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.