MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Chemical Concepts H2O Glue® Aquabonder Underwater Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: H2O Underwater Glue is a toughened structural adhesive used to bond to ABC Plastic, Fiberglass and PVC. The H2O Glue is perfect for repairing pipes, skimmers and main drains. Bonds To: PVC, Fiberglass, ABS, FRT, PBT, PPO, PCBB, Metton®, Lomod®, Valox®, Noryl®, GTX, Minlon®, epoxy, RIM urethane, wood, poorly prepared surfaces, and where outdoor weathering or solvent exposure is anticipated.

Product Features: Minimal surface preparation, Room temperature cure, 1:1mix ratio, Rapid fixture in thin set, Non-sagging formula.

Information provided by Chemical Concepts™.

Vendors:
Available Properties
  • Specific Gravity
  • Density, uncured
  • Solids Content, by volume
  • Volatile Organic Compounds (VOC) Content, mixed
  • pH, 5% solution
  • Viscosity, uncured
  • Viscosity, uncured, activator
  • Viscosity, uncured, adhesive
  • Vapor Pressure
  • Hardness, Shore D, ASTM D 2240
  • Elongation at Break
  • Adhesive Bond Strength, ASTM D1002, vs. ABS
  • Adhesive Bond Strength, ASTM D1002, vs. Polycarbonate
  • Adhesive Bond Strength, ASTM D1002, vs. GBS
  • Peel Strength, ASTM D1876
  • Boiling Point
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Flash Point, uncured
  • Cure Time, Functional
  • Cure Time, Full
  • Working Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.