| The versatile steel that resists wear and abrasion. Hardox 400 is an abrasion-resistant steel with a nominal hardness of 400 HBW. Hardox 400 is a versatile wear-resistant steel. As a result of its high toughness, good bendability and weldability, this steel can be used in structures with moderate wear. Dimension Range: Hardox 400 is available as plate in thicknesses of 4.0 – 130 mm (5/32 - 5.12”), and as sheet in thicknesses of 2.0 - 8.0 mm (0.079 - 0.315”). Hardox 400 plate is available in widths up to 3350 mm (131.89”) and lengths up to 14630 mm (575.98”). Hardox 400 sheet is available in widths up to 1650 mm (64.96”) and lengths up to 16000 mm (629.92”). More detailed information on dimensions is provided in the dimension program. Data provided by SSAB. |