MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Lubrizol Stat-Rite® X-5076 Static Control High Impact Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Stat-Rite® X-5076 is a static dissipative, High Impact Polystyrene alloy. Stat-Rite® X-5076 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protection. Stat-Rite® IDP alloys provide consistent static dissipation properties when thermoformed into complex tray designs. Gardner Drop - Impact Strength is 1.0 in-lb/mil per ASTM D-5420-93.

Features:

  • Superior static decay
  • Clean: no sloughing, low offgassing, low ionics
  • Consistent ESD properties after thermoforming
  • Carbon-free protection

Applications:

  • Electronic component packaging
  • Tape & reel
  • Component handling trays

Properties of all Stat-Rite® polymer products in the molten state are adversely affected by moisture. Although Stat-Rite® compounds are dry when packaged, trace amounts of moisture can be absorbed during storage and handling.

Data provided by Noveon, Inc.

Vendors:
Available Properties
  • Density, ASTM D792
  • Tensile Strength, Yield, ASTM D638-95
  • Elongation at Break, ASTM D638-95
  • Flexural Modulus, ASTM D790-95A
  • Izod Impact, Notched, ASTM D256-92
  • Volume Resistivity, ASTM D257, 50% RH
  • Surface Resistance, ESD S11.11; 50 % R.H.
  • Surface Resistivity per Square, ASTM D257, 50% RH
  • Static Decay, FTMS-101C; 12% R.H., (+5000 V to 50 V)
  • Static Decay, Charged Plate Monitor (+1000 V to 100 V)
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
  • Vicat Softening Point, ASTM D1525-95
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Lubrizol (former Noveon)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.