MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Traid Villarroya TKG® Hgw 2082 Cotton Phenolic Laminate
Categories: Polymer; Thermoset; Phenolic

Material Notes: Laminate manufactured from extra fine and super extra fine cotton mesh impregnated with a phenolic resin binder. It is characterized by its great mechanical strength and low specific gravity. Resilient against a wide variety of chemical agents, it is highly resistant to wear and due to its finer surface, has better machinability than paper grades.

Information provided by Traid Villarroya Hnos. S.L.

Vendors:
Available Properties
  • Density, DIN 53 479
  • Tensile Strength, DIN 53 455
  • Modulus of Elasticity, DIN 53 452
  • Flexural Strength, DIN 53 452
  • Compressive Strength, DIN 53 454
  • Tensile Impact Strength, DIN 53 453, Notched, ak10/ak15
  • Tensile Impact Strength, DIN 53 453, ak10/ak15
  • CTE, linear, VDE 0304
  • Thermal Conductivity, DIN 52 672
  • Maximum Service Temperature, Air, long term
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.