MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Elkem (Bluestar Silicones) SILBIONE® LSR 4330 Liquid Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: Description: SILBIONE® LSR 4330 is a developmental 30 durometer, healthcare grade liquid silicone rubber designed for producing high clarity, high strength molded parts.

Applications:

  • General molded parts
  • Medical applications for <30 day implantation
  • Infant care; baby bottle nipples, pacifiers, sippy cup valves
  • Food contact applications
Features:
  • Superior clarity
  • High tear strength
  • Excellent mold release for shorter cycle times
  • Rapid cure at elevated temperature
  • No post cure is needed

Information provided by Bluestar Silicones

Vendors:
Available Properties
  • Specific Gravity, TP 013
  • Viscosity
  • Viscosity
  • Storage Temperature
  • Hardness, Shore A, ASTM D2240, Press Cured, 5 min, 177°C
  • Hardness, Shore A, ASTM D2240, 4 hr post cure @ 200°C
  • Tensile Strength, ASTM D412, 4 hr post cure @ 200°C
  • Tensile Strength, ASTM D412, Press Cured, 5 min, 177°C
  • Elongation at Break, ASTM D412, 4 hr post cure @ 200°C
  • Elongation at Break, ASTM D412, Press Cured, 5 min, 177°C
  • 100% Modulus, ASTM D412, Press Cured, 5 min, 177°C
  • 100% Modulus, ASTM D412, 4 hr post cure @ 200°C
  • Tear Strength, ASTM D624, Die B, Press Cured, 5 min, 177°C
  • Tear Strength, ASTM D624, Die B, 4 hr post cure @ 200°C
  • Compression Set, ASTM D395B, 4 hr post cure @ 200°C
  • Compression Set, ASTM D395B, Press Cured, 5 min, 177°C
  • Extrusion Rate, TP 001
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.