MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Abatron AboCast/AboCure 8006-11 Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy, Cast, Unreinforced

Material Notes: AboCast/AboCure 8006-11 is a clear dielectric casting, adhesive, and encapsulating compound. It is a 2-component, radiation-resistant, low-viscosity plasticized epoxy system. It is virtually unaffected by atmospheric conditions, soft and salt water, alkalis and diluted acids, several solvents, detergents, oils, and greases. Control of final properties by changing the AboCast/AboCure ratios: the highest rigidity, hardness, chemical and heat resistance are offered by a 100/40 ratio. Higher AboCure ratios (up to 100/100 AboCast/AboCure) yield increasing flexibility, shock and thermocycling resistance, and adhesion to problem surfaces. It has tenacious adhesion to metals, ceramics, wood, fiberglass, masonry, and most materials, to form permanent structural and dielectric bonds. Radiation resistance recommends the 8006-11 System in X-ray and other radioactive environments. Other Suggested Uses: Bonding or laminating substrates, plates lead bricks and other components in radioactive equipment; Dielectric encapsulation and potting of electronic components, especially where high thermocycling and shock resistance are needed; Shrink-free embedments and preparations of specimens for display or analytical purposes; General purpose adhesion, casting, and impregnation.

Vendors:
Available Properties
  • Hardness, Shore A, AboCast/AboCure ratio: 100/100 pbw
  • Hardness, Shore A, AboCast/AboCure ratio: 100/100 pbw
  • Hardness, Shore D, AboCast/AboCure ratio: 100/100 pbw
  • Hardness, Shore D, AboCast/AboCure ratio: 100/80 pbw
  • Hardness, Shore D, AboCast/AboCure ratio: 100/40 pbw
  • Hardness, Shore D, AboCast/AboCure ratio: 100/100 pbw
  • Hardness, Shore D, AboCast/AboCure ratio: 100/80 pbw
  • Tensile Strength at Break
  • Flexural Strength
  • Compressive Strength
  • Izod Impact, Notched
  • Cure Time
  • Cure Time, (1-3 weeks)
  • Pot Life
  • Pot Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.