MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Akrochem ROYALAC™ 150 Curing Agent
Categories: Other Engineering Material

Material Notes: Product Description: ROYALAC™ 150 curing agent is an innovative rubber chemical eveloped by Uniroyal Chemical nd now part of Addivant’s ™ Antioxidant & UV Stabilizer Solutions business. It is an ultra accelerator for natural and synthetic rubbers. It is curing agent offers a variety of common features that are similar to other thiruam disulfide type accelerators such as faster cure and good aging properties. Unique properties to 150 curing agent are improved scorch safety, high elongation, and freedom from bloom. Additionally, articles cured with the curing agent do Not emit nitrosamines. 150 curing agent is available as a liquid or as a 70% active powder.

Application: ROYALAC™ 150 curing agent is effective in a variety of applications. It is an ultra-accelerator and sulfur donor for unsaturated elastomers such as NR, SBR, BR, EPDM and NBR. Vulcanizates using ROYALAC™ 150 curing agent as a partial replacement for sulfur have outstanding high temperature aging properties. ROYALAC™ 150 curing agent has been shown to be successful in co-curing polymer blends of EPDM and NBR as well as SBR/BR blends. ROYALAC™ 150 curing agent is more soluble than other accelerators and is non-blooming even up to 5-7 phr in EPDM. Due to the fact that ROYALAC™ 150 curing agent increases cure rate without sacrificing scorch safety, the addition of ROYALAC™ 150 curing agent can be used to increase productivity. Mounting health and safety concerns, both domestic and abroad, make ROYALAC™ 150 curing agent a responsible choice as nitrosamines are not emitted with its use. Better still, ROYALAC™ 150 curing agent is economical compared to other non-nitrosamine ultra-accelerators. ROYALAC™ 150 curing agent has found utility in rubber compounds for tires, mechanical goods, dense profiles and sponge extrusions.

Information provided by Akrochem Corporation

Vendors:
Available Properties
  • Specific Gravity
  • Flash Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.