MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Polimersan Plastics POLIPA® (PA 6) Polyamide
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: POLIPA® PA6 (POLYAMIDE) is produced by poly condensation of e-aminoacid and by the help of d-carbon acid and d-amine poly condensation. Its characteristics depend upon the numbers of the main structural key carbon atoms, which polyamide contains. Polyamide 66 contains six carbon atoms of d-amine (Hexamethylene d-amine) and six carbon atoms of d-carbonic acid (Adipinacid). This situation is valid also for polyamide 610, which is produced from hexamethyelene d-amine and sabazine acid.

Its composition has significant effect on polyamide properties. Especially, water absorption is mostly affected. As much as CH2-group exists at each CONH-group, water absorption is that much low and dimension accuracy is that very good. (1% humidity absorption equals to 0,3% length elongation.) Parts which are requested to have dimension accuracy at humid atmosphere, are full only with 1.5% water and preferably are made of polyamide 11.(For comparison this value is 10% for PA6.)

Polyamide is preferred as construction material at the conditions where exact measurements are required and which are mechanically loaded like gear wheel, rod, and bolt. Its mechanical properties are significantly dependent on its humidity quantity and degree of crystallization. It can be used also at higher temperatures because of its crystal structure and high melting point. But, when the temperature is higher than 100°C and when there is oxygen at the environment, damage occurs with oxidation. For this reason, for usage at atmosphere only stabilized ones are chosen.

As a result, POLIPA, is a hard plastic due to its high molecular weight and its structure of crosswise bonds. It is resistant to twisting and corrosion. It has the property of working for a long time under load. But, due to its water absorption (9-10%), it is not recommended at humid environments.

CHARACTERISTICS OF POLIPA®:

  • High Mechanical Resistance
  • Hardness and stroke absorption characteristic
  • Electrical Insulation
  • Sliding and high corrosion resistance
  • Resistance to chemicals
GENERAL USAGE AREAS OF POLIPA®:
  • Items which are exposed to loads with strokes
  • Gears
  • Bobbins
  • Vibration Sucking Elements
  • Engineering and maintenance applications with general purpose.

Information provided by Polimersan Polimer Kimya San.Tic.Ltd.Sti.

Vendors:
Available Properties
  • Specific Gravity, ISO.1183 DN.53479
  • Water Absorption, ISO.62 DN.53495
  • Hardness, Rockwell M, ISO.2039-2
  • Hardness, Shore D, DN.53505
  • Ball Indentation Hardness, ISO.2039-2
  • Tensile Strength at Break, ISO.527 DN.53455
  • Tensile Strength, Yield, ISO.527 DN.53455
  • Elongation at Break, ISO.527 DN.53455
  • Modulus of Elasticity, ISO.178 DN.53452
  • Charpy Impact, Notched, ISO.179 DN.53453
  • Volume Resistivity, ISO.167 DN.53482
  • Surface Resistance, ISO.167 DN.53482
  • Dielectric Strength, ISO.243 DN.53481
  • CTE, linear, DN.53752
  • Melting Point
  • Maximum Service Temperature, Air, ISO.75 DN.53461
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic
PA, Polyamide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.