MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
OMG Americas GlidCop® AL-15 Dispersion Strengthened Copper
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Copper Alloy

Material Notes: GlidCop® AL-15 is copper that is dispersion strengthened with 0.3 wt% ultrafine particles of aluminum oxide. It is produced using an internal oxidation powder metallurgy process whereby aluminum oxide is formed in the Cu matrix. The matrix is hardened while the Cu electrical and thermal conductivity are minimally lowered. The aluminum oxide particles are very thermally stable and remain effective in strengthening the copper matrix and resisting grain coarsening even after very long exposures to high temperatures as in brazing or high temp duty cycles.

GlidCop® is available with three different levels of Al2O3. Increasing the Al2O3 levels will increase strength but decrease conductivities. All three grades can be further strengthened by cold work. GlidCop® is available in a wide range of extruded and drawn shapes and sizes, including rounds, rectangles, wire, plates, tubes, and strip. Available on a limited basis in powder form.

Information provided by OMG Americas.

Key Words: OMG Americas; MMC; Metal Matrix Composite
Vendors:
Available Properties
  • Tensile Strength, Yield, With 0% cold work
  • Electrical Resistivity
  • Thermal Conductivity
  • Al2O3
  • Copper, Cu
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.