MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Chesterton ARC I BX1 RC Ceramic-Filled Epoxy/Urethane Industrial Coating
Categories: Polymer; Thermoset; Epoxy; Polyurethane, TS

Material Notes: A rapid curing high impact resistant, 100% solids, epoxy/urethane hybrid with ceramic reinforcements for severe wear regions & impact. ARC I BX1 RC industrial coating is designed to: Cure quickly allowing a faster turn-around with repairs; Coat & protect surfaces exposed to moderate to severe impact & sliding abrasion; Rapidly repair/replace cracked ceramic tile or rubber lining where impact forces combined with sliding wear tear seams and edges; Resist direct and reverse impact forces associated with materials handling system; Easily apply by trowel

Filler: Blend of sintered bauxite beads & SiC powders treated with polymeric coupling agent. Matrix: A modified epoxy/urethane resin hybrid reacted with a fast curing amine curing agent.

Information provided by Chesterton

Vendors:
Available Properties
  • Density, Cured
  • Solids Content
  • Hardness, Shore D, ASTM D2240
  • Tensile Strength at Break, ASTM D638
  • Elongation at Break, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM C580
  • Compressive Strength, ASTM D695
  • Adhesive Bond Strength, ASTM D4541, Pull-Off Adhesion
  • Impact Test, ASTM D2794, Reverse Impact
  • Maximum Service Temperature, Air, Wet Service
  • Maximum Service Temperature, Air, Dry Service
  • Shelf Life, Dry, Unopened Containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.