MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Solvay FM® 6604-1 BMI Foaming Adhesive
Categories: Polymer; Adhesive; Thermoset; Bismaleimide (BMI)

Material Notes: Description: FM® 6604-1 is a modified bismaleimide (BMI) resin core splice foaming adhesive. It has a cure temperature of 350°F (177°C) with a post-cure at 440°C (227°C). The service temperature is -67°F to 450°F (-57°C to 232°C) with post-cure.

Features & Benefits:

  • Maximum continuous service temperature up to 450°F (232°C) with post-cure
  • Expansion ratio 2:1 nominal
  • Ideal for non-metallic core splice and edge closeout
  • Long-term aging
  • Fuel tight
  • High strength-to-density ratio
  • Structural equivalency to unspliced core
Applications:
  • Core shear-ties
  • Edge closeouts
  • Insert bonding

Information provided by Cytec, subsequently acquired by Solvay.

Vendors:
Available Properties
  • Density
  • Volatiles
  • Storage Temperature
  • Shear Strength, Beam
  • Shear Strength, Beam
  • Shear Strength, Tube
  • Shear Strength, Beam
  • Shear Strength, Beam
  • Shear Strength, Tube
  • Shear Strength, Tube
  • Shear Strength, Tube
  • Shear Strength, Tube, 1,1,1 trichloroethane soak per MIL-T-81533 vapor
  • Shear Strength, Tube, 30-day salt spray per ASTM B-117 at 95°F (35°C)
  • Shear Strength, Tube, 72-hour water boil in demineralized water
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay, former Rhodia Engineering Plastics

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.