MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Ovako X20NiCrAlMoV6-5-2-1* Hybrid Steel 60, 397A Steel, Aging, at RT
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: General Information: Hybrid Steel® is a low carbon steel containing a number of carefully controlled alloying elements, most importantly nickel, chromium, aluminium, molybdenum and vanadium. These enable it to develop its full properties after aging at elevated temperature (500–620°C). The chromium and aluminium content also improves corrosion resistance. The variant 297A is offered under the name Hybrid Steel 55 and the variant 397A is offered under the name Hybrid Steel 60.
Hybrid Steel 55 - Engineering steel.
Hybrid Steel 60 - Bearing steel.
Maximum hardness after aging: Hybrid Steel 55, 55HRC. Hybrid Steel 60, 60HRC.

Hybrid Steel offers superior mechanical and fatigue strength compared to conventional steel grades at elevated temperatures.

  • Excellent elevated temperature strength
  • Flexible hardness, achieved by an aging treatment in the temperature range 500–620°C
  • Extremely good dimensional stability when aging is applied
  • High uniformity of properties also for large components
  • Good weldability, no preheating necessary
  • Corrosion resistance comparable to AISI 440C
The density for these grades is 7582 kg/m3.

Information provided by Ovako

Key Words: X20NiCrAlMoV6-5-2-1, X30NiCrAlMoV6-5-2-1 , Ovako297A, Ovako397A
Vendors:
Available Properties
  • Density
  • Tensile Strength, All formats
  • Tensile Strength, Yield, All formats
  • Elongation at Break, All formats
  • Reduction of Area, All formats
  • Modulus of Elasticity
  • Poissons Ratio
  • Shear Modulus
  • Electrical Resistivity
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity, Ambient temperature
  • Transformation Temperature, MS
  • Transformation Temperature, AC1
  • Transformation Temperature, AC3
  • Aluminum, Al
  • Carbon, C
  • Chromium, Cr
  • Iron, Fe, As Balance
  • Manganese, Mn
  • Molybdenum, Mo
  • Nickel, Ni
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  • Vanadium, V
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.