MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger SPI
Ensinger DELRIN® 100AF Acetal Homopolymer, 13% PTFE filled (POM)
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Homopolymer, PTFE-Filled

Material Notes: Ensinger’s DELRIN®100AF blend stock shapes are a 13% PTFE fiber filled homopolymer acetal. They offer an improved coefficient of friction, better lubricity, and improved wear characteristics over unfilled and PTFE powder filled acetals. This advanced acetal material uses a combination of PTFE fibers uniformly dispersed in Delrin acetal resin. The combination results in improved wear characteristics along with strength, toughness, dimensional stability and machinability. The materials exceptional wear properties and internal lubrication serves to reduce or eliminate the need for external lubricants. Ensinger can also produce a full strength 20% PTFE filled version.
  • Excellent wear characteristics
  • Self lubricating
  • Low coefficient of friction
  • Maximum unmodified toughness
  • Superior load bearing characteristics
DELRIN®100AF is often used for applications such as bearing, bushings, cams and other antifriction devices that also require extra toughness.

Information provided by Ensinger

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Density, ASTM D792
  • Water Absorption, ASTM D570
  • Hardness, Rockwell M, ASTM D785
  • Tensile Strength, Yield, ASTM D638
  • Elongation at Yield, ASTM D638
  • Tensile Modulus, ASTM D638, 1mm/min
  • Izod Impact, Notched, ASTM D256
  • Melting Point, ASTM D3418
  • Maximum Service Temperature, Air, long term
  • Maximum Service Temperature, Air, intermittent
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic
POM, Polyoxymethylene

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.