MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Sandvik SAF 2906 Tube and Pipe, Seamless
Categories: Metal; Ferrous Metal; Austenitic

Material Notes: Sandvik SAF 2906 is a high-alloy duplex (austenitic-ferritic) stainless steel with excellent corrosion resistance in caustic environments and environments with chlorides. Sandvik SAF 2906 characteristics::
  • Excellent resistance to caustic environments, also in the presence of contaminants such as chlorides
  • Excellent resistance to intergranular corrosion
  • Excellent resistance to pitting and crevice corrosion
  • High resistance to stress corrosion cracking (SCC)
  • Good weldability
  • Very high strength. The proof strength is about three times as high as for conventional austenitic stainless steels.
Applications:
  • Caustic soda production: the material is suitable for use in piping systems from the cells up to the evaporation plant. It is also an excellent choice for very aggressive conditions, such as the evaporator tubes, in both diaphragm and membrane process.
  • Alumina production: heat exchanger tubes and piping in the digestion of alumina
  • Environments where high resistance to pitting and crevice corrosion is required

Information provided by Sandvik

Key Words: UNS S32906. Comparable to Safurex
Vendors:
Available Properties
  • Density
  • Tensile Strength, Ultimate, Rm
  • Tensile Strength, Ultimate, Rm
  • Tensile Strength, Ultimate, Rm
  • Tensile Strength, Ultimate, Rm
  • Tensile Strength, Ultimate, Rm
  • Tensile Strength, Ultimate, Rm
  • Tensile Strength, Ultimate, Rm
  • Tensile Strength, Ultimate, Rm
  • Tensile Strength, Yield, 300°C
  • Tensile Strength, Yield, 200°C
  • Tensile Strength, Yield, 300°C
  • Tensile Strength, Yield, 200°C
  • Tensile Strength, Yield, 100°C
  • Tensile Strength, Yield
  • Tensile Strength, Yield, 100°C
  • Tensile Strength, Yield
  • Elongation at Break
  • Elongation at Break
  • Elongation at Break
  • Elongation at Break
  • Elongation at Break
  • Elongation at Break
  • Elongation at Break
  • Elongation at Break
  • Modulus of Elasticity
  • Modulus of Elasticity
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Carbon, C
  • Chromium, Cr
  • Copper, Cu
  • Manganese, Mn
  • Molybdenum, Mo
  • Nickel, Ni
  • Nitrogen, N
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.