MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Kohesi Bond KB 1040 LP - FRV Two component, flame retardant epoxy for aircraft interior applications
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive; Epoxy Encapsulant, Unreinforced

Material Notes: Product Highlights:
  • Can pass FAR Standard 14 CFR 25.853 (a)
  • Capable of passing vertical burn test
  • Non-halogen filler
  • Excellent flow properties / can spray paint
  • Color matched to Pantone® Cool Gray 4 C
  • Extremely low smoke generation
Kohesi Bond KB 1040 LP - FRV is a two component, flame retardant, room temperature curing epoxy system suitable for coating, bonding, sealing, potting and encapsulation. It has a 100:30 (Part A: Part B) mix ratio by weight. This flame retardant epoxy is capable of passing the vertical burn test specifications as per Amendment 25-116 and Part 25 Appendix F of the FAR standards. It contains a non-halogenated filler, making it easy to handle and environmentally friendly. The optimum cure schedule for KB 1040 LP - FRV would be an overnight room temperature set-up followed by an addition of heat at 90°C for 3 - 5 hours. KB 1040 LP - FRV offers an extensive service temperature range of -51°C to +121°C. This product’s excellent flow properties and long working time makes it ideal for use in spray coating and casting applications. It offers excellent electrical insulation and excellent chemical resistance to a variety of fuels, oils, common solvents and water. Part A has a gray color and Part B has a white color. Upon mixing, it matches the Pantone® Cool Gray 4 C shade - commonly used for aircraft interiors. KB 1040 LP - FRV’s properties makes it ideal for use in aerospace and aviation related applications, such as door and floor assemblies, interior panels, food trays and electronic potting and sealing.

Typical Applications:

  • Bonding
  • Sealing
  • Coating
  • Potting
  • Encapsulation

Information provided by Kohesi Bond Custom Engineered Adhesives

Vendors:
Available Properties
  • Density, Part B
  • Density, Part A
  • Viscosity, Part B
  • Viscosity, Part A
  • Hardness, Shore D
  • Tensile Strength
  • Tensile Modulus
  • Adhesive Bond Strength, Tensile Lap Shear, Al/Al
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time, Option 2
  • Cure Time, Option 1
  • Working Life, 100 g of mixed epoxy
  • Shelf Life, in original unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.