MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Online Metals
Visit Online Metals for fast service
on small quantity orders.
Alliance BINF-401 Bonded Neo Ferrite Hybrid Magnet
Categories: Ceramic; Oxide; Metal; Electronic/Magnetic Alloy

Material Notes: Hybrid Bonded Magnets made by Compression Molding NdFeB and Ferrite powders with resins such as Nylon 6, Nylon 12 or PPS. The resulting grades have properties that cannot be achieved by typical Ferrite, SmCo or NdFeB sintered and bonded molding processes. Typical usage for a Hybrid magnet is a situation where the application requires more flux than can be provided by a Ferrite magnet but not to the level of a NdFeB magnet.

Information provided by Alliance LLC.

Key Words: Permanent Magnet
Vendors:
Available Properties
  • Density
  • Magnetic Coercive Force, Hc
  • Magnetic Coercive Force, Hc, Intrinsic
  • Magnetic Remanence, Br
  • Magnetic Maximum Energy Product, BH
  • Maximum Service Temperature, Air, Continuous
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Alliance LLC

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.