MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Delphi K-Alloy A304 Casting Alloy
Categories: Metal; Nonferrous Metal; Aluminum Alloy; Aluminum Casting Alloy

Material Notes: Delphi's K-Alloy/A304 is a patented casting alloy engineered to protect today's most critical components from harsh operating environments. It also has high elongation properties when compared to other aluminum die casting alloys.

Benefits

  • Excellent corrosion resistance offers unique engineering solutions
  • High elongation properties
  • Superior finishing quality for high polish applications
  • Better thermal conductivity for improved cooling (15% over A380)
  • Eliminates pre and post processing needs such as anodizing and paint
  • Same castability and flow properties as standard die cast alloys
  • Same shrink factors as existing molds
  • Die life similar to A380
  • No special tooling or process parameters required
Typical Applications
  • Electronic component housings exposed to harsh environments
  • Indoor and outdoor lighting, such as LED lighting
  • Automotive structural components
  • Recreational equipment, such as boats and fishing equipment
  • Defense applications, such as drones, military radios, and antennas
  • Automotive, transportation, and harsh under hood environments

Information provided by Delphi

Vendors:
Available Properties
  • Density
  • Tensile Strength, Heat Treated
  • Tensile Strength, As Cast
  • Tensile Strength, Yield, Heat Treated
  • Tensile Strength, Yield, As Cast
  • Elongation at Yield, As Cast
  • Elongation at Yield, Heat Treated
  • Thermal Conductivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.