MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Master Bond EP30ND Non-Drip, Dimensionally Stable Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: Master Bond Polymer System EP30ND is a high viscosity, two component epoxy adhesive/sealant with a paste consistency. It will cure at room temperature or more rapidly at elevated temperatures and has convenient non-critical 4 to 1 mix ratio by weight or volume. It is 100% reactive and does not contain any diluents or solvents. It is especially useful for applications requiring high bond strength, good chemical resistance along with minimal flow when applied or curing. It is also utilized in many repair applications particularly where machining of cured polymer is desirable. Linear shrinkage is exceptionally low - 0.0003 inches/in. Master Bond Polymer System EP30ND produces high strength bonds that exhibit excellent dimensional stability. Its service temperature range is -60°F to 250°F. It has excellent adhesion to a wide variety of substrates including metals, glass, ceramics, and many plastics. The cured system is a good electrical insulator. The color of part A is amber and the color of part B clear. It is also available in many colors and is especially popular in black. Master Bond Polymer System EP30ND is particularly useful in repair applications involving pumps, pipes, tanks, valves, etc.

Product Advantages:

  • Convenient mixing: easy-to -use mix ratio, four (4) to one (1) by weight or volume.
  • Versatile cure schedules: ambient temperature or fast, elevated temperature cures as required.
  • High bonding strength to similar and dissimilar substrates.
  • Good durability and chemical resistance.
  • Product can be machined or sanded for maximum surface smoothness as desired.
  • Non-drip type system. Easy to apply. Spreads evenly and smoothly.

Information provided by MasterBond®

Vendors:
Available Properties
  • Tensile Strength at Break
  • Compressive Strength
  • Shear Strength, Bond, Al to Al
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • CTE, linear
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time
  • Cure Time
  • Pot Life, 100 gram batch
  • Shelf Life, in unopened container
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.