Features: Excellent combination of strength, stiffness and toughness; Low moisture absorption; Exceptional chemical resistance; Maximum continuous operating temperature 260 °C; Excellent sterilization and hydrolysis resistance; Self-extinguishing, low smoke emission; Pressure nozzle temperature 375°C, printing plate temperature 180°C; Printing room temperature 180°C
Typical Applications: Aviation; Transport; Oil and gas (supporting rings and supply lines
This page displays only the textof a material data sheet.To see MatWeb's complete datasheet for this material (includingmaterial property data, metalcompositions, material suppliers,etc), please click the button below.
Category NotesPlastic