MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Haynes 556® alloy, 40% cold reduction
Categories: Metal; Superalloy; Iron Base

Material Notes: Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists corrosion by molten chloride salts and is resistant to corrosion from molten zinc. Excellent forming and welding characteristics. Applications include tubing and structural members in municipal and industrial waste incinerators, rotary calciners and kilns for minerals processing, and non-rotating components in land-based gas turbines burning low-grade fuels; carbon regenerators, and in processes involving high-sulfur petroleum feedstocks; widely used for hot-dip galvanizing fixtures, spinners, and baskets, high speed furnace fans, air preheaters of diesel engines, the inner covers of coil annealing furnaces, and various high temperature applications in the aerospace industry.

Data provided by the manufacturer, Haynes International, Inc.

Key Words: UNS R30556, AMS 5874, AMS 5877, AMS 5831
Vendors:
Available Properties
  • Density, at RT
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break, in 50.8 mm
  • Modulus of Elasticity, RT
  • Modulus of Elasticity
  • Modulus of Elasticity
  • Modulus of Elasticity
  • Modulus of Elasticity
  • Modulus of Elasticity
  • Modulus of Elasticity
  • Modulus of Elasticity
  • Modulus of Elasticity
  • Modulus of Elasticity
  • Modulus of Elasticity
  • Charpy Impact, Samples did not break. Average of 4 or more tests.
  • Electrical Resistivity, RT
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • Specific Heat Capacity, RT
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Thermal Conductivity, RT
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  • Aluminum, Al
  • Carbon, C
  • Chromium, Cr
  • Cobalt, Co
  • Iron, Fe, As remainder
  • Lanthanum, La
  • Manganese, Mn
  • Molybdenum, Mo
  • Nickel, Ni
  • Nitrogen, N
  • Silicon, Si
  • Tantalum, Ta
  • Tungsten, W
  • Zirconium, Zr
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Haynes International, Inc.

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.